Quality Magazine logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Quality Magazine logo
  • NEWS
  • PRODUCTS
    • SUBMIT YOUR PRODUCT
  • CHANNELS
    • AUTOMATION
    • MANAGEMENT
    • MEASUREMENT
    • NDT
    • QUALITY 101
    • SOFTWARE
    • TEST & INSPECTION
    • VISION & SENSORS
  • MARKETS
    • AEROSPACE
    • AUTOMOTIVE
    • ENERGY
    • GREEN MANUFACTURING
    • MEDICAL
  • MEDIA
    • A WORD ON QUALITY PUZZLE
    • EBOOK
    • PODCASTS
    • VIDEOS
    • WEBINARS
  • EVENTS
    • EVENT CALENDAR
    • QUALITY SHOW
    • IMTS
  • DIRECTORIES
    • BUYERS GUIDE
    • NDT SOURCEBOOK
    • VISION & SENSORS
    • TAKE A TOUR
  • INFOCENTERS
    • NEXT GENERATION SPC & QUALITY ANALYTICS
  • AWARDS
    • ROOKIE OF THE YEAR
    • PLANT OF THE YEAR
    • PROFESSIONAL OF THE YEAR
  • MORE
    • eNEWSLETTER
    • INDUSTRY LINKS
    • THE LEADERSHIP SURVEY
    • CLASSIFIEDS
    • MARKET RESEARCH
    • PRODUCT SPOTLIGHTS
    • QUALITY STORE
    • WHITE PAPERS
    • SPONSOR INSIGHTS
  • EMAG
    • eMAGAZINE
    • ARCHIVES
    • CONTACT
    • ADVERTISE
  • SIGN UP!
NDT

Overview of Fatigue and Creep Testing of Ceramic Matrix Composites for Aerospace

Ceramic Matrix Composites have come a long way in the past decade in their ability to have sustained strength at high temperatures.

By Andrew Harrison, Daniel Traudes
Back2Basics_FT
The extensometer is sitting on a CMC specimen. Source: Exova
Back2Basics_sl2
This is an example of creep frame bearing structure to allow it to meet tight alignment requirements. Source: Exova
Back2Basics_sl3
This is a furnace survey sample. Source: Exova
Back2Basics_sl4
Basic waveform shapes.
Back2Basics_sl5
These are typical creep and fatigue CMC test frames. Source: Exova
Back2Basics_sl6
Back2Basics_sl7
Table of typical properties for ceramics, mild steels and aluminum
Back2Basics_FT
Back2Basics_sl2
Back2Basics_sl3
Back2Basics_sl4
Back2Basics_sl5
Back2Basics_sl6
Back2Basics_sl7
November 9, 2015

Aerospace manufacturers are continually striving to reduce the running costs of their components through reduced weight, improved efficiency or longer service periods, making them more attractive to their market. This can be done by introducing advanced materials, e.g. composites, or improved design, such as sharklet fins on the tips of wings. For aerospace engines this can be done by reducing weight and/or increasing temperatures and pressures.

Recently, this expansion of the performance envelope has been enabled by the introduction of ceramic matrix composites (CMCs) into engine components. CMCs consist of ceramic fibers embedded in a ceramic matrix.

CMCs offer many of the advantages of conventional technical ceramics, namely high melting temperatures, modulus, and hardness. But while conventional ceramics are limited by brittle failure characteristics, low ductility and low fracture toughness, CMCs exhibit increased crack resistance, higher levels of strain to failure and improved thermal shock resistance. Similar to most composites, this is due to the fact that the embedded ceramic fibers in a ceramic matrix allow for a load path through the material even as cracks propagate through the matrix. The subsequent improvement in fracture toughness and ductility allows for the use of CMCs in the high stress, high temperature environment of an engine. Applications within the engine would be items such as combustion chamber liners, stator vanes and turbine blades.

The introduction of any new material into such critical engine items is preceded by an intense period of material testing and evaluation and the fatigue and creep testing methods of CMC materials introduces greater challenges than conventional metals. These two test types are commonly used when defining the allowable and life cycle of an engine.

Engineering fatigue is the repeated application of stress or strain on a component at levels below what would normally cause any permanent deformation or failure. Each application and removal of the applied force is called a cycle and the shape of the load application is the waveform. How fast a cycle is applied is called the frequency. Waveforms can vary, but CMC tests are variants of three basic types.

Creep is the application of a static load at stress levels lower than what would normally cause failure.

For both fatigue and creep testing, damage is built on a microscopic level within the material during test, eventually forming short cracks that lead to fracture as the remaining cross section can no longer support the applied load.

For all materials, sample machining parameters are critical to correctly reproduce surface conditions that accurately represent real components without introducing features that would unrealistically alter the mechanical properties. Additional care must be taken when machining composite coupons from components or panels to avoid delamination which can have a deleterious effect on properties. For CMCs, 3-D CT scanning is generally used to assure the absence of any defects or imperfections that may influence the test results.

In general, because of their use in high temperature areas of an engine, most testing of CMCs is performed in the range of 600 to 1,300 C. This adds complexity to the testing setup as the materials used to manufacture fixture and fittings, normally metallic, are limited to approximately 1,000 C. This has led to a general trend in using low profile furnaces to heat only the critical test section of a CMC test specimen. It requires the gripping to be positioned outside of the furnace and remain warm, permitting the use of lower use temperature metal alloys for fixturing.

Due to the necessity of using warm gripping solutions, the furnace size is minimized so CMC testing has been limited to coupons with relatively short gage lengths and sub-element features.

The low profile CMC furnace uses a different technology to the conventional, which uses coils of wire around a ceramic tube. The CMC has exposed ceramic elements that heat the specimen through radiation and conduction. Due to the small thermal mass of the CMC furnaces, heating rates can be a lot higher, turning heating times to minutes rather than hours. The temperature is controlled to not differ over the duration of a test by more than 3 C for temperatures up to 1,000 C, or more than 6 C for higher temperatures. Additionally, temperature gradients along the critical test section must also be minimized, and will not differ by more than 1% from one area to another.

The furnace is controlled by platinum/platinum-rhodium (R-type) thermocouples, insulated with either mineral or with a ceramic tube. The number and spacing of the thermocouples will depend on the length of the critical test section. However, contact with platinum can lead to chemical reactions with the CMC that will lead to poor test results and so the thermocouples are held close to, but not touching, the specimen surface. Therefore, a furnace survey is conducted with one set of four thermocouples attached to a representative sample, and another set in close approximation to the specimen where they would be located for the test. This allows a correlation between what the test thermocouples read and the actual temperature of the specimen.

Due to the additional complexities in testing composite materials in strain control, CMC testing tends to be in load control with strain monitoring. The strain is monitored through an edge contacting ceramic probe type extensometer.

The strains experienced during CMC testing are small, and the order of magnitude is lower than for metals. Where a typical metallic strain controlled test may be subjected to 0.4% strain, the strains for a CMC will be ~ 0.04%. This means the extensometer has to be very sensitive and calibrated to a low level. Typically, 1% strain is considered full scale for most extensometers.

Care has to be taken when placing the extensometer on the specimen surface as the sharp ends can introduce micro scratches and the uneven nature of CMC surfaces can mean the extensometer can slide during testing, leading to a sudden offset in the test data.

Given the sensitivity of the instrumentation, ambient conditions within the laboratory must be tightly controlled. This not only includes temperature, but air flow and vibration. The extensometers require water cooling to minimize thermal drift and the water flow has to be low flow and must be isolated to avoid strong air currents which can influence strain readings.

Fatigue and creep testing is generally undertaken at the stresses seen by the component in the engine and can vary between 100 to 200 MPa (15 to 30 ksi).

Good load train alignment for axial testing is critical in keeping any bending stresses to a minimum, and previous studies on alignment have shown the detrimental effect on test results. For metallic test pieces, the allowable percentage of bending is defined within the test standard and is usually 5% for fatigue and 10% for creep. However for materials such as CMCs that have low ductility compared to metals, the effects of misalignment can be magnified and subsequently so can the effect on results. Therefore it is usual to have both fatigue and creep allowable percentage bending limited to 3%. This can be achieved by using fixed linear bearings in the loading train.

For fatigue testing, frequencies have to be limited due to the potential of internal friction altering the specimen temperature and taking it outside test tolerance, and are generally between 0.001 and 30 Hz. However, extensometry is limited to lower frequency testing due to extensometer stability on the rougher CMC surface topography.

Various test information can be recorded and supplied depending on customer requirements. Load, displacement, strain and temperature can be logged and these can be used to generate load/strain/temperature against cycle plots or load against strain/displacement loop plots.

Test durations are dependent on a variety of factors relating to the material properties and test conditions. Some tests may last only seconds, while others could last from hours to days to weeks. Because of these extended timescales, long-term stability of laboratory ambient environmental conditions are critically important. In addition, an uninterruptable power supply (UPS) should be used to allow continued running, or controlled shut down, of a test frame.

As with most composite materials, the failure mechanism in tension generally initiates at a micro level in the matrix. Once the matrix and fibers begin to lose intimate contact, this can then lead to fiber pull-out, delamination and a net tension failure.

Ceramic Matrix Composites have come a long way in the past decade in their ability to have sustained strength at high temperatures. However there is still a considerable amount of characterization required to develop a database to allow these materials to be considered “airworthy.” As CMCs continue to evolve, so will the need to continue these types of high temperature tests to suit their applications.

KEYWORDS: aerospace testing fatigue testing

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Andrew Harrison is a technical manager.For more information, please email [email protected], call +44 (0) 7827280119 or visit www.exova.com

Daniel Traudes is the fatigue laboratory manager at Exova Anaheim. For more information, visit www.exova.com

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • 2024 Quality Rookie of the Year Justin Wise 1440x750px banner with "Quality Rookie of the Year" logo inset

    Meet the 2024 Quality Rookie of the Year: Justin Wise

    Justin Wise is an exceptional individual who has been...
    Aerospace
    By: Michelle Bangert
  • Man with umbrella and coat stands outside while it rains at night looking at a building.

    Nondestructive Testing: Is there an ethics problem?

    I was a whistleblower who exposed fraudulent activities...
    NDT
    By: Dale Norwood
  • Unraveling Deflategate: Football stadium with closeup of football on field

    Unraveling the Tom Brady Deflategate

    The Deflategate scandal erupted following the 2014 AFC...
    Measurement
    By: Greg Cenker and Henry Zumbrun
Subscribe For Free!
  • eMagazine Subscriptions
  • eNewsletters
  • Online Registration
  • Subscription Customer Service
  • Manage My Preferences

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the Quality audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of Quality or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • image: Meeting in a conference room, all three people looking at an ipad.
    Sponsored byInnovMetric

    Your Manufacturing Process Deserves Digitally Connected 3D Measurement Data

Popular Stories

Technician working with the Vision Engineering LVC200.

Difference Between Calibration and Verification

Woman working in quality control, measuring a workpiece.

AI’s Double-Edged Sword: Security and Compliance in Manufacturing

QM0525-FEAT-A3-Automation-p1FT-Quality-Inspection.jpg

The Next Frontier of Automation: Quality Assurance in an AI-Driven Era

April 29 Quality Advantive Live Webinar

Events

April 29, 2025

When AI Meets SPC: Unlocking Even More Value From Your SPC Quality Data

Discover how SPC's real-time data collection, monitoring and control capabilities provide the perfect foundation for AI/ML's predictive insights, enabling both immediate process optimization and long-term continuous improvement.

May 21, 2025

The Evolution of Laser Radar: Measuring Large Scale From Distance With High Accuracy

This webinar, featuring a live demonstration, will showcase the evolution of Hexagon’s direct scanning laser trackers: cutting-edge technology that now delivers traditional reflector-tracking accuracy to non-contact, large-part scanning.

View All Submit An Event

Products

Lean Manufacturing and Service Fundamentals, Applications, and Case Studies

Lean Manufacturing and Service Fundamentals, Applications, and Case Studies

See More Products
Play Quality's captivating word-guessing game! There's a new word every Friday.

Related Articles

  • TestingMetals_FT

    Testing Metals and Advanced Materials in Aerospace

    See More
  • Continuous ceramic fibers

    Continuous Ceramic Fibers Let CMCs and MMCs Take Off in Aerospace and Other Industries

    See More
  • DEPT101_FT

    Mechanical Testing of Composites

    See More

Related Products

See More Products
  • ZEuCDwAAQBAJ.jpg

    Lean Six Sigma In The Age Of Artificial Intelligence: Harnessing The Power Of The Fourth Industrial Revolution

  • funds of manu cell.gif

    Fundamentals of Manufacturing Cell Planning DVD Package

  • fundamentals of plant fl.jpg

    Fundamentals of Plant Floor Layout DVD Package

See More Products

Events

View AllSubmit An Event
  • May 15, 2024

    Mastering Ultrasonic Testing Inspection of Small-Bore Welds: Unveiling the Power of 2D Matrix Arrays

    On Demand Join us for an insightful webinar on optimizing Phased Array Ultrasonic Testing (PAUT) inspection of small-bore welds with 2D matrix arrays.
View AllSubmit An Event

Related Directories

  • American Institute of Nondestructive Testing

    The American Institute of Nondestructive Testing offers online and hands-on training in RT, UT, ET, MT, PT and VT nondestructive testing methods. Let us customize an NDT training program that fits your company's needs. We offer training online, at your facility or at our 22,000 Sq Ft facility.
×

Stay in the know with Quality’s comprehensive coverage of
the manufacturing and metrology industries.

eNewsletter | Website | eMagazine

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • eNewsletter
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Market Research
    • Reprints
    • List Rental
    • Survey/Respondent Access
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • YouTube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2025. All Rights Reserved BNP Media.

Design, CMS, Hosting & Web Development :: ePublishing